Measurement of residual stress on TiN/Ti bilayer thin films using average X-ray strain combined with laser curvature and nanoindentation methods Journal article
MATERIALS CHEMISTRY AND PHYSICS, 2017,Volume: 199,Page: 185-192
Authors:  Lei, Soichan;  Huang, Jia-Hong;  Chen, Haydn
Favorite |  | TC[WOS]:8 TC[Scopus]:7 | Submit date:2018/10/30
Ti interlayer  TiN  Residual stress  Average X-ray strain  Synchrotron X-ray