Micro-mechanical properties of calcium sulfoaluminate cement and the correlation with microstructures Journal article
Cement and Concrete Composites, 2017,Volume: 80,Page: 10-16
Authors:  Hu C.;  Hou D.;  Li Z.
Favorite |  | TC[WOS]:31 TC[Scopus]:34 | Submit date:2019/04/08
Calcium sulfoaluminate cement  Composition  Micro-mechanical properties  Microstructure