Property investigation of individual phases in cementitious composites containing silica fume and fly ash Journal article
Cement and Concrete Composites, 2015,Volume: 57,Page: 17-26
Authors:  Hu C.;  Li Z.
Favorite |  | TC[WOS]:56 TC[Scopus]:62 | Submit date:2019/04/08
Calcium silicate hydrate  Fly ash  Mechanical properties  Microstructure  Silica fume