Nanohardness of nanocrystalline TiN thin films Journal article
Surface and Coatings Technology, 2006,Volume: 200,Issue: 12-13,Page: 3868-3875
Authors:  Ma C.-H.;  Huang J.-H.;  Chen H.
Favorite |  | TC[WOS]:78 TC[Scopus]:81 | Submit date:2019/04/08
Nanohardness  Residual stress  Texture  TiN