Characterisation of the interfacial transition zone in mortars by nanoindentation and scanning electron microscope Journal article
Magazine of Concrete Research, 2018,Volume: 70,Issue: 18,Page: 965-972
Authors:  Gao Y.;  Hu C.;  Zhang Y.;  Li Z.;  Pan J.
Favorite |  | TC[WOS]:6 TC[Scopus]:6 | Submit date:2019/04/08
Cement  Cementitious materials  Modulus of elasticity  Mortar  
Investigation on microstructure and microstructural elastic properties of mortar incorporating fly ash Journal article
Cement and Concrete Composites, 2018,Volume: 86,Page: 315-321
Authors:  Gao Y.;  Hu C.;  Zhang Y.;  Li Z.;  Pan J.
Favorite |  | TC[WOS]:15 TC[Scopus]:18 | Submit date:2019/04/08
Characterization  Elastic properties  Fly ash  Interfacial transition zone  Microstructure  Mortar  
Measurement of residual stress on TiN/Ti bilayer thin films using average X-ray strain combined with laser curvature and nanoindentation methods Journal article
MATERIALS CHEMISTRY AND PHYSICS, 2017,Volume: 199,Page: 185-192
Authors:  Lei, Soichan;  Huang, Jia-Hong;  Chen, Haydn
Favorite |  | TC[WOS]:8 TC[Scopus]:7 | Submit date:2018/10/30
Ti interlayer  TiN  Residual stress  Average X-ray strain  Synchrotron X-ray  
Quantitative characterization and elastic properties of interfacial transition zone around coarse aggregate in concrete Journal article
Journal Wuhan University of Technology, Materials Science Edition, 2017,Volume: 32,Issue: 4,Page: 838-844
Authors:  Jia Z.;  Han Y.;  Zhang Y.;  Qiu C.;  Hu C.;  Li Z.
Favorite |  | TC[WOS]:9 TC[Scopus]:12 | Submit date:2019/04/08
backscattered electron image  concrete  elastic modulus  interfacial transition zone  nanoindentation  
Micro-mechanical properties of calcium sulfoaluminate cement and the correlation with microstructures Journal article
Cement and Concrete Composites, 2017,Volume: 80,Page: 10-16
Authors:  Hu C.;  Hou D.;  Li Z.
Favorite |  | TC[WOS]:31 TC[Scopus]:34 | Submit date:2019/04/08
Calcium sulfoaluminate cement  Composition  Micro-mechanical properties  Microstructure  
Statistical nanoindentation technique in application to hardened cement pastes: Influences of material microstructure and analysis method Journal article
Construction and Building Materials, 2016,Volume: 113,Page: 306-316
Authors:  Hu C.;  Gao Y.;  Zhang Y.;  Li Z.
Favorite |  | TC[WOS]:26 TC[Scopus]:27 | Submit date:2019/04/08
Composition  Hardened cement paste  Mechanical properties  Micromechanics  Microstructure  Statistical analysis  
Estimation of the poroelastic properties of calcium-silicate-hydrate (C-S-H) gel Journal article
Materials and Design, 2016,Volume: 92,Page: 107-113
Authors:  Hu C.;  Gao Y.;  Chen B.;  Zhang Y.;  Li Z.
Favorite |  | TC[WOS]:9 TC[Scopus]:9 | Submit date:2019/04/08
Calcium-silicate-hydrate gel  Micromechanics  Poroelastic properties  
Micromechanical investigation of magnesium oxychloride cement paste Journal article
Construction and Building Materials, 2016,Volume: 105,Page: 496-502
Authors:  Hu C.;  Xu B.;  Ma H.;  Chen B.;  Li Z.
Favorite |  | TC[WOS]:27 TC[Scopus]:31 | Submit date:2019/04/08
Magnesium oxychloride (MOC) cement  Micromechanical properties  Microstructure  Multiscale modeling  
Property investigation of individual phases in cementitious composites containing silica fume and fly ash Journal article
Cement and Concrete Composites, 2015,Volume: 57,Page: 17-26
Authors:  Hu C.;  Li Z.
Favorite |  | TC[WOS]:54 TC[Scopus]:61 | Submit date:2019/04/08
Calcium silicate hydrate  Fly ash  Mechanical properties  Microstructure  Silica fume  
Residual stress measurement on TiN thin films by combing nanoindentation and average X-ray strain (AXS) method Journal article
Surface and Coatings Technology, 2015,Volume: 280,Page: 43-49
Authors:  Wang A.-N.;  Huang J.-H.;  Hsiao H.-W.;  Yu G.-P.;  Chen H.
Favorite |  | TC[WOS]:13 TC[Scopus]:15 | Submit date:2019/04/08
Average X-ray strain (AXS)  Cos2αsin2ψ method  Nanoindentation  Residual stress  TiN thin film