Selected(0)Clear
Items/Page: Sort: |
| Cavitation erosion of a spinodally decomposed wrought duplex stainless steel in a benign environment Journal article Wear, 2019,Volume: 424-425,Page: 111-121 Authors: Wenji Ai; K.H. Lo ; C.T. Kwok
 Favorite | View/Download:99/0 | TC[WOS]:1 TC[Scopus]:2 | Submit date:2019/03/25 Cavitation Erosion Duplex Stainless Steel Spinodal Decomposition Tensile |
| Spindle speed in friction surfacing of 316L stainless steel – How it affects the microstructure, hardness and pitting corrosion resistance Journal article Surface and Coatings Technology, 2019,Volume: 361,Page: 324-341 Authors: D. Guo; C.T. Kwok; S.L.I. Chan
 Favorite | View/Download:13/0 | TC[WOS]:6 TC[Scopus]:13 | Submit date:2019/02/14 Austenitic Stainless Steel Dynamic Recrystallization Friction Surfacing Hardness, Pitting Corrosion |
| Enhancement in hardness and corrosion resistance of AISI 420 martensitic stainless steel via friction stir processing Journal article Surface and Coatings Technology, 2019,Volume: 357,Page: 339-347 Authors: L. Pan; C.T. Kwok ; K.H. Lo
 Favorite | View/Download:17/0 | TC[WOS]:6 TC[Scopus]:11 | Submit date:2019/02/14 Corrosion Friction Stir Processing Hardness Martensitic Stainless Steel |
| Fabrication of stainless steel 316L/TiB2 composite coating via friction surfacing Journal article Surface and Coatings Technology, 2018,Volume: 350,Page: 936-948 Authors: D. Guo; C.T. Kwok ; S.L.I. Chan
 Favorite | View/Download:13/0 | TC[WOS]:8 TC[Scopus]:13 | Submit date:2019/02/14 Crystallography Friction Surfacing Metal Matrix Composite Pitting Corrosion Stainless Steel Titanium Diboride |
| Post-fire mechanical and corrosion properties of duplex stainless steel: Comparison with ordinary reinforcing-bar steel Journal article CONSTRUCTION AND BUILDING MATERIALS, 2018,Volume: 174,Page: 150-158 Authors: Xiang Li; K.H. Lo ; C.T. Kwok ; Y.F. Sun; K.K. Lai
 Favorite | View/Download:29/0 | TC[WOS]:2 TC[Scopus]:6 | Submit date:2018/10/30 Duplex Stainless Steel Post-fire Property Spinodal Decomposition Tensile Behaviour Pitting Behaviour |
| Effect of laser surface melting and subsequent re-aging on microstructure and corrosion behavior of aged S32950 duplex stainless steel Journal article MATERIALS CHEMISTRY AND PHYSICS, 2018,Volume: 207,Page: 451-464 Authors: W.K. Chan; C.T. Kwok ; K.H. Lo
 Favorite | View/Download:34/0 | TC[WOS]:3 TC[Scopus]:6 | Submit date:2018/10/30 Laser Surface Modification Aging Corrosion Duplex Stainless Steel |
| Implications of solution treatment on cavitation erosion and corrosion resistances and synergism of austenitic stainless steel Journal article WEAR, 2017,Volume: 392-393,Page: 159-166 Authors: K.H. Lo ; C.T. Kwok ; K.Y. Wang; Wenji Ai
 Favorite | View/Download:55/0 | TC[WOS]:10 TC[Scopus]:13 | Submit date:2018/10/30 Cavitation Erosion Austenitic Stainless Steel Martensitic Transformation Solution Treatment Corrosion |
| Laser fabrication of W-reinforced Cu layers: I. Corrosion behavior in 3.5% NaCl solution and synthetic acid rain Journal article Materials Chemistry and Physics, 2016,Volume: 181,Page: 397-408 Authors: P.K. Wong; C.T. Kwok ; H.C. Man; D. Guo
 Favorite | View/Download:6/0 | TC[WOS]:2 TC[Scopus]:5 | Submit date:2019/02/14 Alloys Coatings Corrosion Sem |
| Laser surface alloying of copper with titanium: Part I. Electrical wear resistance in dry condition. Part II. Electrical wear resistance in wet and corrosive condition Journal article Surface and Coatings Technology, 2016,Volume: 297,Page: 58-73 Authors: C.T. Kwok ; P.K. Wong; H.C. Man
 Favorite | View/Download:15/0 | TC[WOS]:0 TC[Scopus]:9 | Submit date:2019/02/14 Electrical Sliding Wear Hardness Intermetallic Phases Laser Surface Alloying |
| Laser fabrication of W-reinforced Cu layers: II. Electrical wear behavior in air and synthetic acid rain Journal article Materials Chemistry and Physics, 2016,Volume: 177,Page: 118-130 Authors: P.K. Wong; C.T. Kwok ; H.C. Man; D. Guo
 Favorite | View/Download:11/0 | TC[WOS]:2 TC[Scopus]:3 | Submit date:2019/02/14 Composites Copper Electrical Wear Laser Surface Modification Tungsten Wear-corrosion Synergism |